该文通过对红锥和西南桦人工林木材南北向、不同高度位置、不同径向位置横向干缩 (包括弦、径向 )的测量 ,讨论分析了以上 3个因素对上述两种木材横向干缩率的影响 .研究结果表明 ,南北向的不同对红锥和西南桦人工林木材的干缩均无显著影响 ;高度位置的不同对红锥径、弦向干缩影响均不显著 ,而对西南桦径、弦向干缩的影响极为显著 ;径向位置的不同对红锥人工林木材的径、弦向干缩及西南桦的弦向干缩无显著影响 ,但对西南桦的径向干缩则有极显著影响 .

红锥和西南桦人工林木材应用于家具装饰材的初步研究

格式:pdf

大小:384KB

页数: 5页

In this paper,the related properties(long-term dimensional stability,adhesion strength,painting film adhering capacity,painting film wearing and consuming value and wood surface hardness) of two plantation-grown hardwoods(Betula alnoides and Castanopsis hystrix),compared with commonly used Quercus mongolia domestically,were investigated. The test on long-term dimensional stability is referred to the method established by New Zealand Forest Research Institute,test on adhesion strength is conducted according to the criteria ASTM D905-89,the test on painting film adhering capacity is referred to the criteria GB/T 1765-1999 and GB/T 1765-1999,and wood surface hardness is referred to JIS Z2117-1963.In the meantime,adhesion strength and painting film adhering capacity are assigned to the corresponding grades according to different criterion based on a series of experimental results. The results show as follows: the adhesion strength,painting film adhering capacity of B. alnoides,C. hystrix and Q. mongolia belong to excellent grade with similar long-term dimensional stability. The total of radial and tangential swelling coefficient of the three species are 0.064%,0.068% and 0.066%,respectively. With regard to painting film wearing and consuming value of the three species,the quality grades are good,middle and good in order. The surface hardness on different wood surfaces of three species is 11.0,7.7 and 13.0 MPa on radial surface,14.2,10.6 and 12.5 MPa on tangential surface,33.0,26.6 and 38.1 MPa on end surface,respectively.

热门知识

红桦

精华知识

红桦

最新知识

红桦
点击加载更多>>
红桦相关专题

分类检索: